Alloys
Technical alloy data

CuSn8 strip and coil

CuSn8 is a high-tin phosphor bronze for spring connectors requiring higher strength while retaining reasonable thermal stability.

Standards: ASTM B888

Phosphor bronze

CuSn8 phosphor bronze

CuSn8 | C52100 | CW453K | PB104 ≈ C52100 (CW453K)

Spring connectorsSignal transmission contactsHigh spring-force parts
01

Chemical composition

Sn8 %
Curemainder
02

Physical properties

Property Metric Imperial
Electrical conductivity7.5 MS/m13 % IACS
Thermal conductivity62 W/(m.K)36 Btu.ft/(ft2.h.deg F)
Coefficient of electrical resistance0.7 10^-3/K0.4 10^-3/deg F
Coefficient of thermal expansion18.2 10^-6/K10.1 10^-6/deg F
Density8.80 g/cm30.318 lb/in3
Modulus of elasticity110 GPa16,000 ksi
Specific heat0.377 J/(g.K)0.090 Btu/(lb.deg F)
Poisson's ratio0.340.34
Temper range

Mechanical properties

Structured values for quote review, engineering checks and PDF generation.

Standard Temper Rm MPa Rm ksi Rp0.2 MPa Rp0.2 ksi A50 % Hardness Grain size mm
Chart data

Performance snapshots

Graph series are generated from the same alloy technical config used for the PDFs.

Forms

Dimensions

Tempers