Chemical composition
Sn4 %
Curemainder
CuSn4 combines cold formability, strength, reasonable electrical conductivity, and useful thermal stability for stamped and bent electronic components.
Standards: ASTM B888
CuSn4 | C51100 | CW450K | PB101 (close) ≈ C51100 (CW450K)
| Property | Metric | Imperial |
|---|---|---|
| Electrical conductivity | 13 MS/m | 22 % IACS |
| Thermal conductivity | 84 W/(m.K) | 48 Btu.ft/(ft2.h.deg F) |
| Coefficient of electrical resistance | 1.3 10^-3/K | 0.7 10^-3/deg F |
| Coefficient of thermal expansion | 17.8 10^-6/K | 9.9 10^-6/deg F |
| Density | 8.85 g/cm3 | 0.320 lb/in3 |
| Modulus of elasticity | 120 GPa | 17,500 ksi |
| Specific heat | 0.377 J/(g.K) | 0.090 Btu/(lb.deg F) |
| Poisson's ratio | 0.34 | 0.34 |
Structured values for quote review, engineering checks and PDF generation.
| Standard | Temper | Rm MPa | Rm ksi | Rp0.2 MPa | Rp0.2 ksi | A50 % | Hardness | Grain size mm |
|---|
Graph series are generated from the same alloy technical config used for the PDFs.