Chemical composition
Sn6 %
Curemainder
CuSn6 is a spring-capable phosphor bronze for stamped connectors and press-fit pins where formability, strength, conductivity, and thermal stability matter.
Standards: ASTM B103
CuSn6 | C51900 | CW452K | PB103 ≈ C51900 (CW452K)
| Property | Metric | Imperial |
|---|---|---|
| Electrical conductivity | 10 MS/m | 17 % IACS |
| Thermal conductivity | 75 W/(m.K) | 43 Btu.ft/(ft2.h.deg F) |
| Coefficient of electrical resistance | 0.7 10^-3/K | 0.4 10^-3/deg F |
| Coefficient of thermal expansion | 18.0 10^-6/K | 10.0 10^-6/deg F |
| Density | 8.80 g/cm3 | 0.318 lb/in3 |
| Modulus of elasticity | 118 GPa | 17,000 ksi |
| Specific heat | 0.377 J/(g.K) | 0.090 Btu/(lb.deg F) |
| Poisson's ratio | 0.34 | 0.34 |
Structured values for quote review, engineering checks and PDF generation.
| Standard | Temper | Rm MPa | Rm ksi | Rp0.2 MPa | Rp0.2 ksi | A50 % | Hardness | Grain size mm |
|---|
Graph series are generated from the same alloy technical config used for the PDFs.