Chemical composition
Cu63 %
Znremainder
CuZn37 is an economical brass for moderate strength, moderate conductivity, and excellent formability.
Standards: ASTM B36
CuZn37 | C27200 | CW508L | CZ108 ≈ C27200 (CW508L)
| Property | Metric | Imperial |
|---|---|---|
| Electrical conductivity | 15 MS/m | 26 % IACS |
| Thermal conductivity | 120 W/(m.K) | 69 Btu.ft/(ft2.h.deg F) |
| Coefficient of electrical resistance | 1.7 10^-3/K | 0.9 10^-3/deg F |
| Coefficient of thermal expansion | 20.2 10^-6/K | 11.2 10^-6/deg F |
| Density | 8.44 g/cm3 | 0.305 lb/in3 |
| Modulus of elasticity | 105 GPa | 15,000 ksi |
| Specific heat | 0.377 J/(g.K) | 0.090 Btu/(lb.deg F) |
| Poisson's ratio | 0.34 | 0.34 |
Structured values for quote review, engineering checks and PDF generation.
| Standard | Temper | Rm MPa | Rm ksi | Rp0.2 MPa | Rp0.2 ksi | A50 % | Hardness | Grain size mm |
|---|
Graph series are generated from the same alloy technical config used for the PDFs.