Chemical composition
Cu79-81 %
Znremainder
Ni0.3 max %
Sn0.1 max %
Fe0.05 max %
Pb0.05 max %
Al0.02 max %
CuZn20 has excellent cold formability and good hot formability. The alloy has higher strength than pure copper. CuZn20 has good welding and hard-soldering properties as well as good corrosion resistance, and is not susceptible to stress corrosion or dezincification.
Standards: ASTM B36/B36M
CuZn20 | C24000 | CW503L | CZ103
| Property | Metric | Imperial |
|---|---|---|
| Melting point | 965-1000 deg C | |
| Density | 8.67 g/cm3 | |
| Specific heat | 0.38 kJ/(kg.K) | |
| Thermal conductivity | 142 W/(m.K) | |
| Electrical conductivity | >=32.8 % IACS | |
| Modulus of elasticity | 119 GPa | |
| Coefficient of thermal expansion | 18.8 10^-6/K |