Chemical composition
Sn0.1 %
Curemainder
CuSn0.15 increases mechanical stability and softening resistance while retaining high conductivity and excellent formability.
Standards: ASTM B152/B152M
CuSn0.15 | C14415 | CW117C
| Property | Metric | Imperial |
|---|---|---|
| Electrical conductivity | 51 MS/m | 88 % IACS |
| Thermal conductivity | 350 W/(m.K) | 202 Btu.ft/(ft2.h.deg F) |
| Coefficient of electrical resistance | 3.2 10^-3/K | 1.8 10^-3/deg F |
| Coefficient of thermal expansion | 18.0 10^-6/K | 10.0 10^-6/deg F |
| Density | 8.93 g/cm3 | 0.323 lb/in3 |
| Modulus of elasticity | 125 GPa | 18,000 ksi |
| Specific heat | 0.385 J/(g.K) | 0.092 Btu/(lb.deg F) |
| Poisson's ratio | 0.34 | 0.34 |
Structured values for quote review, engineering checks and PDF generation.
| Standard | Temper | Rm MPa | Rm ksi | Rp0.2 MPa | Rp0.2 ksi | A50 % | Hardness | Grain size mm |
|---|
Graph series are generated from the same alloy technical config used for the PDFs.