Chemical composition
Cu>=99.90 %
Pb0.005 max %
P0.005-0.013 %
Bi0.0005 max %
CuDLP is a deoxidised, low-phosphorus oxygen-free copper with very good formability and joining properties. Conductivity is lower than pure copper but higher than Cu-DHP and Cu-HCP because of the reduced phosphorus content.
Standards: ASTM B152/B152M
CuDLP | C12000 | CW023A | C106 (close)
| Property | Metric | Imperial |
|---|---|---|
| Melting point | 1083 deg C | |
| Density | 8.94 g/cm3 | |
| Specific heat | 0.377 kJ/(kg.K) | |
| Thermal conductivity | 350 W/(m.K) | |
| Electrical conductivity | >=90 % IACS | |
| Modulus of elasticity | 132 GPa | |
| Coefficient of thermal expansion | 17.7 10^-6/K |
Structured values for quote review, engineering checks and PDF generation.
| Standard | Temper | Rm MPa | Rm ksi | Rp0.2 MPa | Rp0.2 ksi | A50 % | Hardness | Grain size mm |
|---|
Graph series are generated from the same alloy technical config used for the PDFs.